【2KG Pack】Blue PETG 1kg 3D Printer Filament

In stock
Regular price $49.00
Warehouse
Size

Use this text to encourage communication or promote sharing on social networks.

You can also add links

PETG (Polyethylene Terephthalate)-a co-polyester known for durability and wide range of uses, The G in PETG means the filament is glycol-modified.which gives it a clear and glass like properties. Each spool contains 1 kg (2.2 lbs) of filament.

Clog-Free & Bubble-Free | Less-tangle and Easy to Use | Dimensional Accuracy & Consistency

Recommended parameters for PETG printing:
Filament Diameter: 1.75mm.
Tolerance: +/- 0.02mm.
Recommended Extrusion / Nozzle Temp: 210 - 230℃ (410℉~ 446℉).
Heated Bed Temp: 70 - 80℃(158℉~176℉).
Print Speed: 25-30m/s.
Density: 1.25±0.05g/cm3
Filament Length: 335m

Package includes:

Blue PETG 1kg * 2 rolls / 6 rolls / 10 rolls

FREE shipping from our US / EU / Australia / Mexico / Chinese / UK warehouses.
The picture is for reference only. Please adhere to the original products in case of any mistakes.

Filament Specifications:
1.75mm +/- 0.05mm in diameter

Recommended Print Settings:
• Extruder Temperature: 210-235℃, recommended temp 220℃
• Bed temperature: 50-80℃
• Fan Speed: 100%
• Printing Speed: 30-70mm/s
• Heated Bed: Required
• Recommended Build Surfaces: Masking Paper, PVP Soild Glue, PEI
• Print Suggestion: Drying at 65℃ />3h

More information of PETG

CLICK HERE
PLA PETG Rapid PLA
RECOMMENDED NOZZLE TEMP: 190°C - 220°C
(recommended 205°C)
220-260°C
(recommended 220°C)
200-230°C
(recommended 220°C)
RECOMMENDED HEATED BED TEMP: 50-65°C 50-80°C 40-60°C
PRINTING SPEED: 30~70mm/s 30~70 mm/s 30~600 mm/s
PRINT LAYER THICKNESS: 0.2mm 0.2mm 0.2mm
RECOMMENDED PLATFORM: Glass/Fiberglass Board/PVP glue stick or textured paper Glass/Fiberglass Board/PEI+PVP glue stick or platform spray Glass/Fiberglass Board/PEI+PVP glue stick or platform spray
DIMENSIONAL ACCURACY 99% PROBABILITY: +/- 0.02mm +/- 0.02 mm +/- 0.02 mm
NET WEIGHT: 1 kg/spool (2.2 lbs) 1 kg/spool (2.2 lbs) 1 kg/spool (2.2 lbs)
DENSITY: 1.2(g/cm³) 1.27(g/cm³) 1.2(g/cm³)
TENSILE STRENGTH (X-Y) : ≥ 50(MPa) ≥60(MPa) ≥60(MPa)
ELONGATION AT BREAK (X-Y) : 11.2 (%) 19 (%) 19 (%)
BENDING MODULUS : 1913(MPa) 2680(MPa) 2680(MPa)
BENDING STRENGTH : 91(MPa) 80(MPa) 80(MPa)
CHARPY IMPACT STRENGTH : 5.4(kJ/m²) 3.85 (KJ/m²) 3.85 (KJ/m²)
MELT INDEX: 14(190℃/2.16kg)g/10min 8.2(190°C/2.16kg)g/10min 8.2(190°C/2.16kg)g/10min
THERMAL DISTORTION TEMP: 53°C (0.45MPa) 53°C (0.45MPa) 53°C (0.45MPa)
FAN: 100% 100% 100%
ROCKWELL HARDNESS: 88 88 88